Items | Co-extruded WPC | Normal WPC |
Color: | Rich, vivid,strong steady leveling natural wood color | Single solid color and the very few thickness oxidation |
Anti-scratch | Stronger | Better than wood |
Expansion rate | Lower,about 0.1% | About 0.3-0.5% |
Water absorption | Smaller only the two ends | Better than wood |
Weathering test | Much stronger | Better than wood |
Water/oil stain | N/A | May occasionally occur |
Cleaning Method | Water, very easy | Sand paper,steel wool etc |
Wood grain | Never disappears | May be not very clear |
Mold stain | N/A | Better than wood |
Test Method | Test Item | Result | |
ISO 4892-2 | Xenon Arc Weathering | Non-exposure | 2000h Exposure |
ISO 4892-2 | Color Change | - | Gray Scale 3 |
ISO 178 | Flexural Strength Flexural Modulus |
26.3Mpa 2.44Gpa |
25.0 Mpa, decrease 4.9% 2.24GPa,decrease 8.2% |
ISO 179 | Impact Strength | 4.86KJ/square meter | 4.66KJ/square meter,decrease 4.1% |
Test Method | Characters | Result |
ASTM D638 | Tensile test | 18.0Mpa |
ASTM E831 | Coefficient of linear thermal expansion | 40.5 μm/mC |
ASTM D256 | Impact resistance | 33.7J/m Type of break: Complete Break |
ASTM D6109 | Flexural strength | MOR:29.3Mpa MOE:3715Mpa |
ASTM D790 | Flexural properties | MOR:34.1Mpa MOE:2503Mpa |
ASTM D4060 | Abrasion resistance | Weight loss: 0.07g |
ASTM D6007 | Formaldehyde test | ND² |
Country | Sales Quantity in 2017 |
France | 1000sqm |
America | 9000sqm |
Brazil | 7000sqm |
Canada | 6500sqm |
Bulgaria | 5500sqm |
Romania | 9800sqm |
Thailand | 4900sqm |
India | 8600sqm |